Improve the performance of piezoelectric ceramic sheets, such as increasing their electromechanical coupling coefficient and reducing dielectric loss, to meet the requirements of high-precision and high-efficiency applications. Develop piezoelectric ceramic devices with multiple functions, such as temperature compensation and frequency filtering, to meet various complex application requirements. Adopting environmentally friendly materials and manufacturing processes to reduce environmental pollution and resource waste, while improving product reliability and safety. By combining microelectronics technology and artificial intelligence technology, intelligent control and optimized design of piezoelectric ceramic sheets can be achieved, improving their performance and energy efficiency. Advance manufacturing processes and technologies to achieve miniaturization and miniaturization of piezoelectric ceramic sheets, in order to meet the needs of portable electronic devices and micro machinery.
Typ | Fr(Kiloherth) | (k31)% | C(PF) | d3310-12(CN) | Tg(%) |
PLS-P51-151110 | 70±5% | 30 | 4680±10% | 500 | 2 |
PLS-P51-201615 | 50±5% | 30 | 9700±10% | 500 | 2 |
PLS-P51-252115 | 39±5% | 35 | 12400±10% | 500 | 2 |
PLS-P51-292520 | 34±5% | 35 | 19400±10% | 550 | 2 |
PLS-P51-302518 | 33±5% | 35 | 14250±10% | 550 | 2 |
PLS-P51-322820 | 36±5% | 35 | 21600±10% | 550 | 2 |
PLS-P51-343020 | 28±5% | 35 | 23000±10% | 550 | 2 |
PLS-P51-383225 | 26±5% | 35 | 21000±10% | 550 | 2 |
PLS-P51-403237 | 25±5% | 35 | 24000±10% | 550 | 2 |
PLS-P51-453925 | 22±5% | 35 | 25200±10% | 550 | 2 |
PLS-P51-504425 | 19±5% | 35 | 28200±10% | 550 | 2 |
PLS-P51-553930 | 19±5% | 35 | 33800±10% | 550 | 2 |
PLS-P51-605430 | 16±5% | 35 | 41000±10% | 550 | 2 |
PLS-P51-655930 | 15±5% | 35 | 44600±10% | 550 | 2 |
PLS-P51-756716 | 13±5% | 35 | 20400±10% | 550 | 2 |
PLS-P51-807420 | 12±5% | 35 | 36900±10% | 550 | 2 |
PLS-P51-908420 | 10±5% | 35 | 52180±10% | 550 | 2 |